When Teal-Jones Lumber, a member of the Teal-Jones Group, purchased Langdale Lumber in Antlers, Okla., in late 2014, it carried on its parent company’s tradition of providing customers with top-quality wood products.

Aerial view of the Teal-Jones mill in Antlers, Oklahoma, with rows of pine logs in the yard

Mill worker in a hard hat checking boards on a conveyor lineThe Oklahoma mill manufactures dimensional Southern Yellow Pine lumber, which is used in a wide range of building applications because of its strength, dependability, and versatility. Pine logs come to the mill from the surrounding area. At the mill, they’re cut, dried, and planed, and the lumber is sold to wholesalers throughout the United States and parts of Mexico.

On average, Teal-Jones produces 50 million board feet a year. In 2016, when this article was written, the mill was expecting record production.

The process for producing quality products and ensuring consistent grading standards is rigorous at Teal-Jones Lumber. Each piece is inspected and graded for knots, bark remnants, slope of grain, and material efficiency to meet or exceed all standards.

إدارة الرطوبة أمر بالغ الأهمية

It’s in the mill’s two double-track kilns, each capable of drying 125,000 board feet per charge, that consistent quality is maintained.

“To help minimize warping and shrinkage associated with green lumber, our Southern Pine is kiln dried for long-term stability,” says Kerry Cogburn, Teal-Jones Kiln Supervisor.

“In fact, our kiln drying is critical to our success. In order to produce high quality products, it’s extremely important that we know the moisture content (MC) throughout the drying process because if we overdry or underdry the wood, we can downgrade it,” he adds.

To dry the lumber properly, Teal-Jones uses the MC4000 In-Kiln Moisture Measurement System from Wagner Meters. Installed in the mill’s two kilns, the MC4000 works in tandem with American Wood Dryers’ Drystar Computer Control System. The Drystar takes the information from the MC4000 and tells the kilns what to do: heat up or cool down, adjust the dry bulb or wet bulb, and open the vents.

As a kiln supervisor, Cogburn says تجفيف الفرن is an art that requires skill and technical knowledge. “But having a dependable in-kiln moisture measurement system working together with the Drystar computer system makes it that much easier,” he says.

وهناك أيضًا ميزة اقتصادية كبيرة.

“By having the in-kiln system, we don’t have to shut the kiln down several times, open it up, and lose all that heat. We rely on the Wagner system to tell us when our 2x products reach our target range of 19% MC and our 4x products hit 24% MC. It’s very costly to bring the kilns back up to 200°F or so.”

بتقليل فحوصات الحرارة إلى فحص واحد، أو ربما فحصين لكل شحنة، لا نفقد تلك الحرارة. وهذا يوفر لنا الطاقة. في الواقع، أقدر أن ذلك يوفر لنا 300,000 دولار سنويًا، وذلك بفضل توفير الوقت وتكاليف الطاقة والجهد المبذول في تجفيف الخشب.

مواجهة التحدي

When the MC4000 says the wood is done, kiln operators confirm it with مسبار قياس أكوام الأخشاب من واغنر L722 attached to the L622 digital recording moisture meter. The challenge is leaving the right amount of moisture in the wood so it isn’t overdried or underdried.

Kiln operator holding a stack probe into a stack of kiln-dried pine with a handheld meter

A kiln operator uses Wagner’s L722 Lumber Stack Probe.

“That’s where the L622 and the stack probe comes in handy. When the magical number (MC) comes up with the MC4000, they’ve been consistently reliable in confirming our wood is ready,” Cogburn says.

In the past, the mill used a pin meter to see if the charge was ready, but that proved unreliable and costly.

باستخدام مقياس الدبابيس، قد نضطر لبدء الشحن مرتين أو ثلاث مرات قبل أن نحصل على النتيجة المطلوبة. يُغني جهاز L622 ومسبار المكدس عن ذلك، كما يقول.

بالإضافة إلى ذلك، يقوم جهاز L622 بمهمة أخرى لم يكن بمقدور مقياس الدبابيس القيام بها. فهو يسمح لنا بتنزيل ملخص تقرير مُفصّل على جهاز كمبيوتر يمكننا طباعته. سيُعطيني هذا مُتوسط قراءات الرطوبة المُسجلة، والرسوم البيانية، ونسبة الرطوبة الكلية لكل شحنة. لذا، فقد كان أداة قيّمة للغاية بالنسبة لنا.

Moisture management is critical for Teal-Jones Lumber, especially during kiln drying. “It’s what has helped us produce quality lumber consistently and efficiently,” says Cogburn.

"والأهم من ذلك، أن يكون ذلك مربحًا أيضًا."

The Teal-Jones Group describes itself as the largest privately held forest products company operating on the West Coast of Canada.

تحديث المنتج: لم يعد مقياس الرطوبة L622 المذكور في هذه المقالة متوفرًا. وقد تم استبداله بـ جهاز قياس رطوبة الخشب المحمول الصناعي L5300, which works with the L722 Lumber Stack Probe.